ZINC 300

• Provides good protection against corrosion from atmospheric influences
• Resistance up to approximately 300 ºC
• Visually identical to hot galvanizing
• Two or three coats on the repaired surface will provide the required layer of thickness according to D.I.N. 50976
• Fast drying (dust dry after approximately 15 minutes; fully dry after approximately 6-3 days)
• Surface has to be dust, grease, and rust free according to D.I.N. 55928, up to the derusting degree SA 2.5 and must also be dry
ZINC 300
• Provides good protection against corrosion from atmospheric influences
• Resistance up to approximately 300 ºC
• Visually identical to hot galvanizing
• Two or three coats on the repaired surface will provide the required layer of thickness according to D.I.N. 50976
• Fast drying (dust dry after approximately 15 minutes; fully dry after approximately 6-3 days)
• Surface has to be dust, grease, and rust free according to D.I.N. 55928, up to the derusting degree SA 2.5 and must also be dry
 
Application:
• The layer thickness of the repair film should be 1.5 times that of hot galvanizing
• The repair coat should overlap the hot galvanizing area by at least 1 cm
• Can be welded through
• Can be applied with a paint gun, airless, or with a brush
• Cannot be over-painted
 
Application area:
• Steel construction, ship building, forging, locksmiths, and vehicle building